It is considered thatpropagation of crack width was mitigated because some crackswere developed in different parts of slabs near the interiorsupport. Accordingly, it is considered that the appropriate crackwidth control initially at transverse joints is more important.Load–relative slip curves were also measured experimen-tally through the static loading test performed up to 900 kNafter the repeated loading test (Fig. 24). The increase of rela-tive slip provokes the increase of deflection and the occurrence of cracks in the concrete deck at the internal support may alsoaffect the increase of deflection. Also, the difference of longi-tudinal stiffness in bridges due to the development of cracksin the deck may influence the occurrence of relative slip. Fur-ther analytical researches are expected to help the examinationof this subject. In general, it is considered that the test spec-imen could be also assumed with full composite action until900 kN loading after one million cyclic loading, because moni-tored slips were relatively smaller than ultimate slip of the shearconnection [6,7].Fig. 21. Load–deflection curves under static loading up to 900 kN.Fig. 25 plots the maximum strains (strain at the bottomflange) in the maximum positive moment section and in thenegative moment section of the girder measured until 900 kN.In view of the level of the developed strains, the girder remainsin the elastic range up to the load of 900 kN. In the result, thenonlinear behaviour of the whole bridge can consequently beunderstood as caused mainly by the cracking developed in theconcrete deck. Moment curvature relationship of the bridge model up to900kN loading was also reached as shown in Fig. 26. Inthe maximum negative moment section, the propagation ofcracking in the slab on the interior support makes the stiffnessdecrease. Although cracking of bottom slabs happens at loadingpoints and top slabs on the interior support, the curve of themaximum positive moment section was nearly maintained asthe curve of uncracked composite section (Fig. 26) where girderdid not reach yielding (Fig. 25). In the maximum negativemoment section, the stiffness of the bridge model decreasedgradually and similarly traced the curve evaluated by Eurocode4-2 after design cracking load. However, with moment increase,the stiffness of the composite girder was largely decreasedand eventually became equal to that of cracked compositesection as shown in Fig. 26. It can be observed that the flexuralstiffness of the negative moment section in the test modellargely decreased compared to the effective stiffness calculatedusing Eurocode 4-2 as a result of cyclic loading. It is suggestedthat bonding between reinforcement and concrete becomesweak due to repeated loading effects and thus tension stiffeningeffects decrease. Nevertheless, it is considered that momentcurvature relationship or the flexural stiffness by Eurocode 4-2is still useful for estimation of the effective stiffness consideringtension stiffening effects in the composite bridge with loopjoints prefabricated slabs.

摘要为研究裂缝控制,选取了一个带有预制板的两跨连续组合双肋梁的足尺模型,并对其进行试验及观察。在试验中,第一次荷载加到360kN,然后进行疲劳荷载试验。最后静力加载至900kN。试验结果证实了带预制板的双肋连续组合梁显示出了在静力疲劳荷载作用下的组合截面的强度和刚度特性。然而,在负弯矩作用区域,裂缝集中在内部支撑之上的桥面之间的接缝部位,初始的裂缝间距由接缝处间的距离决定,在使用荷载作用下,带有预制板的组合桥梁的桥面和横向接缝的裂缝宽度可以被控制在一个容许裂缝宽度之内。弯矩曲率曲线或者由欧洲规范4-2中规定的抗弯刚度仍可被用于评估考虑到在这种桥梁上拉伸硬化作用的有效刚度。源:自*优尔~·论,文'网·www.youerw.com/

c 2007 Published by Elsevier Ltd 

毕业论文关键词:裂缝控制;连续组合双梁桥;预制板;环缝;横向接头;静力疲劳载荷;组合截面复合截面的负弯矩区;裂缝宽度;抗弯刚度

上一篇:CAD知识的模具设计英文文献和中文翻译
下一篇:抗侧向荷载的结构体系英文文献和参考文献

数控机床制造过程的碳排...

新的数控车床加工机制英文文献和中文翻译

抗震性能的无粘结后张法...

锈蚀钢筋的力学性能英文文献和中文翻译

未加筋的低屈服点钢板剪...

汽车内燃机连杆载荷和应...

审计的优化管理英文文献和中文翻译

我国风险投资的发展现状问题及对策分析

麦秸秆还田和沼液灌溉对...

张洁小说《无字》中的女性意识

互联网教育”变革路径研究进展【7972字】

网络语言“XX体”研究

老年2型糖尿病患者运动疗...

安康汉江网讯

新課改下小學语文洧效阅...

ASP.net+sqlserver企业设备管理系统设计与开发

LiMn1-xFexPO4正极材料合成及充放电性能研究